埋弧焊是一种以电弧为热源,在焊接状态下进行电弧燃烧的焊接方法。由于弧焊熔深、生产率高、机械化程度高,适用于中厚板结构的焊缝。埋弧焊是当今焊接生产中应用最广泛的焊接方法之一,但只能在平焊位置进行焊接。

Submerged arc welding is a kind of welding method which takes the arc as the heat source and carries out arc combustion in the welding state. Due to the deep penetration, high productivity and high degree of mechanization of arc welding, it is suitable for welds of medium and heavy plate structure. Submerged arc welding is one of the most widely used welding methods in welding production, but it can only be welded at the flat welding position.

埋弧焊的主要焊接参数有:焊接电流、电弧电压、焊接速度、焊丝直径和焊丝伸出长度等。埋弧焊的焊接材料包括焊丝和焊剂,其选择应根据母材的力学性能和化学成分、坡口形式、厚度、工艺条件和结构尺寸等。低合金钢和低碳钢可以选择与钢材强度相匹配的焊丝和焊剂,同时还应满足其他标准要求。选用碳钢H08A、H08MnA焊丝,选用高锰高硅焊剂,或选用H08MnA、H10Mn2焊丝,匹配低猛无锰型焊剂。

The main welding parameters of submerged arc welding include: welding current, arc voltage, welding speed, wire diameter and wire extension length. The welding materials for submerged arc welding include welding wire and flux, which shall be selected according to the mechanical properties and chemical composition of the base metal, groove form, thickness, process conditions and structural dimensions. Welding wire and flux matching with steel strength can be selected for low alloy steel and low carbon steel, and other standard requirements shall be met at the same time. Carbon steel H08A and H08MnA welding wires, high manganese and high silicon flux, or H08MnA and H10Mn2 welding wires, matched with low fierce manganese free flux.

低合金高强度钢应使用低合金高强度钢焊丝,在选用中猛中硅或低锰中型冶炼熔剂时也可使用烧结熔剂。

Low alloy high strength steel welding wire shall be used for low alloy high strength steel, and sintering flux can also be used when medium fierce medium silicon or low manganese medium smelting flux is selected.

耐热钢的焊接,应选择成分与钢相似的焊接。对于熔剂的选择,可选用低温耐热钢和耐腐蚀钢作为碱性中硅或低硅型剂,应选用高碱度合金钢或烧结结合焊等高合金钢,以减少合金元素的燃烧,增加更多的合金元素。此外,还应考虑各种技术因素的影响。

For the welding of heat-resistant steel, the welding with composition similar to that of steel shall be selected. For the selection of flux, low-temperature heat-resistant steel and corrosion-resistant steel can be selected as alkaline medium silicon or low silicon type flux, and high-alloy steel such as high alkalinity alloy steel or sintering bonding welding shall be selected to reduce the combustion of alloy elements and increase more alloy elements. In addition, the influence of various technical factors should also be considered.

焊丝的表面质量,如直径偏差、表面硬度、曲率均匀性等,都会影响焊接过程的稳定性和焊接质量。因此,加载前应检查焊丝,并消除折弯。使用前应干燥,焊剂粒度影响透气性,对焊缝成形和内部质量有一定影响。在焊剂尺寸不变的情况下,如果增加焊接电流,电弧会不稳定,焊缝表面和边缘会不平整,电流越大,焊剂粒度应越大。

The surface quality of welding wire, such as diameter deviation, surface hardness and curvature uniformity, will affect the stability and quality of welding process. Therefore, the welding wire shall be checked and the bending shall be eliminated before loading. Dry before use. The particle size of flux affects the air permeability and has a certain impact on the weld formation and internal quality. When the flux size remains unchanged, if the welding current is increased, the arc will be unstable and the weld surface and edge will be uneven. The larger the current is, the larger the flux particle size should be.

焊接速度对熔宽和熔深有影响。在其他条件不变的情况下,焊接速度随着焊缝接速度的增加而显著减小。电弧向后倾角的增大有利于熔池金属的流动,因此深度略有增加。

The welding speed has an effect on the width and depth of penetration. When other conditions remain unchanged, the welding speed decreases significantly with the increase of welding speed. The increase of arc backward angle is conducive to the metal flow in the molten pool, so the depth increases slightly.

相关文章

为什么涂料老是开裂(为何家里的乳胶漆总是容易出现开裂)

近年来,许多人在墙面装修的时候,都会选择刷乳胶漆,乳胶漆颜色丰富,耐脏和耐擦洗性出色,实用性高。但是,为何有的人家里的乳胶漆总是容易出现开裂,经过有老师傅提醒,才发现原来是这5点没做好。1、墙面粘结强度不够许多人在房屋刷乳胶漆后,老是出现开裂和空鼓,这主要因为墙面粘结强度不够,建议大家,将原先的墙皮

2025-05-12 23:48:02

为什么防漏电插座不会漏电(从功能上识别插座安全性)

安全插座到底要如何选择?选择什么样的安全插座才能保证儿童安全?现在市场上安全插座五花八门,个个都声称是“安全插座”,这给广大家长们在选购中带来了不少困扰,众所周知,市面上所谓的“安全插座”其实并不安全。伪劣产品众多。这也严重威胁儿童的用电安全。前段时间央视《每周质量报告》节目也曾对当前市场上的插座安

2025-05-12 22:58:21

大红酸枝木为什么开裂(买了大红酸枝家具,偶尔听到炸响怎么办?)

买了大红酸枝家具,偶尔听到炸响怎么办?其实大红酸枝家具炸想属于正常现象。那是红木家具开裂发出的声音,不必大惊小怪。小编在网上查看到很多用户在购买大红酸枝家具之后,发现家具会有炸响的现象,这到底是怎么一回事呢?下面我们一起来看看其中的原因以及维修的方法:红酸枝家具之所以容易开裂炸响,主要是因为红酸枝属

2025-05-12 22:55:32

为什么墙身瓷砖脱落(墙上的墙砖老是掉,还是要讲点道理)

墙砖被师傅贴在墙上,时间没到过多久,就出现很多墙砖掉落,甚至有些还会大面积出现脱落的现象。有不少人的房主不知道其缘由,事后就会将所有的原因全部怪在贴砖师傅身上,责任是否真的如房主所想呢?责任的归属,对于这行业有接触过的人,都还是有着一定的了解,施工人员的正确施工,确实对瓷砖脱落,有着一定的关系,但也

2025-05-12 22:40:24

水泵为什么频繁启动(自吸泵怎么吸不出来水)

1自吸泵怎么吸不出来水自吸泵抽不出水的原因及排除方法:自吸泵在使用的过程中,有时会出现不出水的问题。这就需要找出具体原因加以排除。造成自吸泵抽不出水的原因及排除方法有以下三种可能性:1-1 自吸泵体内无引水或存水不足。只有自吸泵的泵体内存有一定量的水,才能在起动。因旋转时的叶轮所产生的离心力将进水管

2025-05-12 20:32:27

为什么有暗卫的房子(为什么豪宅多暗卫?)

日常在和朋友的交流中,朋友提出最多的问题就是高端户型中为什么会有这么多的暗卫,在产品研发的过程中能够避免吗?今天就对这个问题进行简要的分析。一、主次功能房间的划分要求暗卫产生的最主要原因,是因为豪宅户型面积过大,且面宽有限,进深过长,因此在户型内部就形成了一些“暗角”,相比于对采光通风要求更高的客餐

2025-05-12 20:23:59